This highly plastic clay is ideal for reduction firing but is also suitable for oxidation and may be salt-glazed. It has excellent resistance to warping and cracking and the high proportion of ball clay in this body makes it a real pleasure to work with. Ideal for the production of domestic tableware.
Firing Temp 1220-1300°C